In this episode I attempt to explain Galvanic Corrosion, as I need to add another Zinc Anode to fully protect the bronze propeller. After more antifouling paint we enjoy some extremely satisfying tape-peeling, and finally we relaunch Tally Ho and do some manoeuvring to test how the boat handles with a freely moving rudder